Submerged Arc Furnace
n Application:
mainly used for reducing smelting ore, carbon reductant and solvent etc, producing ferrosilicon, ferromanganese, ferrochrome, ferrotungsten, silicon-manganese alloy etc
类别
Furnace Type
|
主要原料
Main Material
|
制成品
Product
|
反应温度
Reaction Temperature
(℃)
|
电耗
Power Consumption (KWh/Ton)
|
Ferrosilicon (45%)
|
ferrosilicon, iron scrap, coke
|
ferrosilicon
|
1550-1770
|
2100-5500
|
Ferrosilicon (75%)
|
ferrosilicon, iron scrap, coke
|
ferrosilicon
|
1550-1770
|
8000-11000
|
Ferromanganese
|
manganese ore, iron scrap, coke, lime
|
ferromanganese
|
1500-1400
|
2400-4000
|
Ferrochrome
|
chrome ore, silica,
coke
|
ferrochrome
|
1600-1750
|
3200-6000
|
Ferrotungsten
|
tungsten ore,
coke
|
ferrotungsten
|
2400-2900
|
3000-5000
|
Silicon-chromium
|
ferrochrome, silica, coke
|
silicochromium alloy
|
1600-1750
|
3500-6500
|
Silicon-manganese
|
manganese ore, silica, iron scrap, coke
|
silicomanganese alloy
|
1350-1400
|
3500-4000
|
Steel-making
|
iron ore,
coke
|
pig iron
|
1500-1600
|
1800-2500
|
Calcium Carbide
|
limestone,
coke
|
calcium carbide
|
1900-2000
|
2900-3200
|
Boron Carbide
|
boron
oxide
|
boron carbide
|
1800-2500
|
about 2000
|
Remarks:
|
The power consumption greatly varies due to furnace capacity and composition of material and product, the valued indicated here is only for reference purpose.
|
n
|